Chromium is plated from acidic dichromate according to Cr₂O₇²⁻ + 14H⁺ + 12e⁻ → 2Cr(s) + 7H₂O. How many hours are required to plate a 0.25 m² bumper to thickness 2.0 × 10⁻² mm at 75.0 A? Take chromium density 7.19 g
Chemistry · Electrochemistry · Electrolysis: Electrolytic reactions, electrode processes, Faraday's laws, and quantitative calculations.
Chromium is plated from acidic dichromate according to Cr₂O₇²⁻ + 14H⁺ + 12e⁻ → 2Cr(s) + 7H₂O. How many hours are required to plate a0.25 m² bumper to thickness 2.0 × 10⁻² mm at 75.0 A? Take chromium density 7.19 g cm⁻³, M(Cr) = 52 g mol⁻¹, F = 96500 C mol⁻¹ and 100% current efficiency.
Options
Related questions
- Which listed ion promotes iron corrosion in an acidic aqueous environment?
- Select the correct statements about the conventional standard hydrogen electrode reference (SHE).
- One faraday is the amount of charge :
- The temperature coefficient of the cell is ( ∂ E ∂ T ) P \left(\frac{\partial E}{\partial T}\right)_{P} ( ∂ T ∂ E ) P . Choose the corr…
- During electrolysis of aqueous CuBr₂ using Pt electrode,
- Two compartments of an electrolytic cell each contain 100 mL buffer with 1 M NH₃ and 1 M NH₄⁺. The left electrode is the anode and the righ…